Logo image
Help Advanced Search
Artificial intelligence based analysis of nanoindentation load–displacement data using a genetic algorithm
Journal article   Open access   Peer reviewed

Artificial intelligence based analysis of nanoindentation load–displacement data using a genetic algorithm

Abraham Burleigh, Miu Lun Lau, Megan Burrill, Daniel T. Olive, Jonathan G. Gigax, Nan Li, Tarik A. Saleh, Frederique Pellemoine, Sujit Bidhar, Min Long, …
Applied surface science, Vol.612, p.155734
03/01/2023

Abstract and subjects

Artificial intelligence Genetic algortithm Nanoindentation
url
https://doi.org/10.1016/j.apsusc.2022.155734View
Published (Version of record) Open

Metrics

16 Record Views

Details